MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

USI Corporation UNITHENE® LH606 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: UNITHENE® LH606 is a high density polyethylene resin (HDPE) for use in injection molding and fine monofilament.

Characteristics:

  • Good environmental stress cracking resistance
  • High impact strength
  • Excellent stiffness
  • High hardness
  • Great surface gloss
  • Less warpage
  • Low shrinkage
Main Application:
  • Fruit crates, transportation crates, housewares
  • Food containers
  • Mosquito nets

Information provided by USI Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.962 g/cc0.0348 lb/in³ASTM D792
Melt Flow 6.0 g/10 min6.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6969ASTM D2240
Tensile Strength, Yield 30.4 MPa4410 psiASTM D638
Elongation, Ultimate 600 %600 %ASTM D638
Flexural Yield Strength 95.2 MPa13800 psiASTM D747
1% Secant Modulus 971 MPa141000 psiMolded; ASTM D638
Izod Impact, Notched 0.686 J/cm1.29 ft-lb/inASTM D256
Torsional Stiffness 1230 MPa178000 psiASTM D1043
 
Thermal PropertiesMetricEnglishComments
Melting Point 135 °C275 °FASTM D3418
Vicat Softening Point 127 °C261 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FF50; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PUSIC030 / 285398

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.