MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Wacker Silpuran® 6400/40 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Liquid silicone rubber of the SILPURAN® 6400 series is a paste-like, easily-pigmentable two-component compound with short curing times. Their vulcanizates are noted for their high transparency and excellent mechanical and electrical properties. Especially they are noted for an excellent tear resistance according to ASTM D 624 B and DIN ISO 34-1 Method A (DIN 53507).

Properties: SILPURAN® 6400/40 A/B meets selected test requirements of ISO 10993 and United States Pharmacopoeia (USP) Class VI. Postcured parts can be used for food contact applications and are suitable for use under the Recommendation "XV. Silicones" of the BfR and FDA § 177.2600 under observance of any given limitations on extractable and volatile substances.

Special features: A master file has been filed with the U.S. Food and Drug Administration.

Application: SILPURAN® 6400/40 A/B is particularly suitable for the economical production of large series of injection-moulded articles. SILPURAN® 6400/40 A/B is designed for medical and pharmaceutical applications including implantation for < 30 days.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³DIN EN ISO 1183-1 A
Viscosity  375000 cP
@Shear Rate 10.0 1/s
375000 cP
@Shear Rate 10.0 1/s
DIN 53019
 830000 cP
@Shear Rate 1.00 1/s
830000 cP
@Shear Rate 1.00 1/s
DIN 53019
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040DIN 53505
Tensile Strength at Break 9.20 MPa1330 psiDIN 53505 S1
Elongation at Break 630 %630 %DIN 53505 S1
Tear Strength 15.0 kN/m85.6 pliDIN ISO 34-1 method A
 35.0 kN/m200 pliASTM D624B
Compression Set 20 %
@Temperature 175 °C,
Time 79200 sec
20 %
@Temperature 347 °F,
Time 22.0 hour
DIN ISO 815-B
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %"Transparent" but manufacturer does not quantify.
 
Processing PropertiesMetricEnglishComments
Cure Time  5.00 min
@Treatment Temp. 165 °C
0.0833 hour
@Treatment Temp. 329 °F
postcuring for 4 h/200 °C in ventilated air.
 5.00 min
@Treatment Temp. 165 °C
0.0833 hour
@Treatment Temp. 329 °F
postcuring for 6 h/200 °C in ventilated air.
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
Colortransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Silpuran® 6000/40 A/B Liquid Silicone Rubber
Wacker Silpuran® 6740/40 A/B Liquid Silicone Rubber
Wacker ELASTOSIL® R plus 4105/40 Solid Silicone Rubber-Batch Grade

PWACK9492 / 205021

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.