MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Momentive Performance Materials GE Silicones RapidStrength RGS7700 Two-Component, Fast Curing Silicone Elastomeric Adhesive
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: RGS7700 silicone elastomeric adhesive is a two-component, 100% silicone neutral cure sealant that rapidly builds adhesive and elastomeric strength for bedding and glazing of glass in residential and commercial window designs.

Features: Silicone Durability, Adhesion Performance, Structural Capability.

Applications: RGS7700 is an excellent candidate to consider as bedding or glazing adhesive where fast green strength and cure speed facilities movement of assemblies on high speed production lines.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccuncured cayalyst RGS7700B
 1.19 g/cc
 1.35 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 28
Tensile Strength, Ultimate 1.58 MPaASTM D412
Tensile Stress at Strain 0.340 MPa
@Strain 50 %
ASTM D412
 0.760 MPa
@Strain 100 %
ASTM D412
Elongation, Ultimate 280 %ASTM D412
Peel Strength 51.21 pliASTM C794
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °FHeat Resistance
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 12.0 - 36.0 min
Shelf Life 12.0 Monthcatalyst RGS7700B.
 18.0 Month
 
Descriptive Properties
Accelerated WeatheringExcellent, no degradation.ASTM C1369. 5000 hrs.
AppearanceThixotropic PasteAs supplied, uncured cayalyst RGS7700B
 Thixotropic PasteAs supplied, uncured.
 Thixotropic PasteMixed
ColorBlackAs supplied, uncured cayalyst RGS7700B
 GrayCured
 GrayMixed, RGS7700A+RGS7700B
 Gray, black, white, beige, custome color available.Depends on curing agent.
 Off whiteuncured.
Consistency / Sag<0.05”Mixed, RGS7700A+RGS7700B, non-sagging.
Cyclic Movement Capacity+/- 50%
Green Strength Tensile100 psi60 minute Cure. ASTM C1135
 15 psi15 minute Cure. ASTM C1135
Mix Ratio10:1 by volumeAs Tested
 8:1 to 12:1
Snap Time6-18 minutes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9920 / 265730

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.