MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound EC004APQ Polyetherimide (PEI)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: LNP THERMOCOMP EC004APQ compound is based on Polyetherimide (PEI) resin containing 20% carbon fiber. Added features of this grade include: Electrically Conductive, FAR25.853 Compliant.

Features: FAR 25.853 Compliant,High Stiffness,Light-weight Structural,High Heat Resistance,Super Strong (Carbon Fiber Filled),Electrically Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
 0.150 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 - 0.0070 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 245 MPa5 mm/min; ASTM D638
Elongation at Break 2.3 %5 mm/min; ASTM D638
Tensile Modulus 19140 MPa5 mm/min; ASTM D638
Flexural Strength 344 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 15800 MPa1.3 mm/min, 50 mm span; ASTM D790
Poissons Ratio 0.44ASTM E132
Shear Modulus 4.399 GPaASTM D732
Shear Strength 121.35 MPaASTM D732
Izod Impact Notched 109 JASTM D256
Izod Impact, Unnotched 711 J/mASTM D4812
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1e+05 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 5.40 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 55.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 170 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 390 - 400 °C
Zone 2 370 - 390 °C
Zone 3 380 - 400 °C
Melt Temperature 360 - 400 °CInjection Molding
Mold Temperature 140 - 180 °C
Drying Temperature 150 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa
Vent Depth 0.00250 - 0.00760 cm
 
Descriptive Properties
Screw speed (Circumferential speed)0.2-0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81570 / 289517

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.