MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Skydrol® LD4 Fire Resistant Hydraulic Fluid
Categories: Fluid

Material Notes: Product Description: Skydrol LD-4 was introduced in 1977 , and is well known around the world. At the time of its introduction it was a breakthrough product, solving problems of valve erosion and thermal stability common in earlier fluids. Its excellent thermal stability under real world conditions has given it a reputation as the gold standard among Type IV fluids. Skydrol LD-4 features low density, excellent thermal stability, valve erosion prevention, and deposit control.

Application/Uses:

  • Aviation hydraulic systems

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.003 - 1.013 g/cc
Viscosity Measure 3.66 - 4.0 cSt
@Temperature 99.0 °C
 10.65 - 11.65 cSt
@Temperature 38.0 °C
 <= 2000 cSt
@Temperature -54.0 °C
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.10[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Pour Point <= -62.0 °C
Flash Point >= 160 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %
 
Descriptive Properties
AppearanceClear, oily liquid
ColorPurple
Content<10 ppmCalcium
 <10 ppmSodium
 <30 ppmPotassium
 <50 ppmChlorine
 1185-1540 ppmSulfur
Fire Point>177°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay RHODAFAC® LO-11/ALA Surfactant
Eastman Skydrol® PE-5 Fire Resistant Hydraulic Fluid
Eastman Skydrol® 500B-4 Fire Resistant Hydraulic Fluid

PEATM5584 / 222778

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.