MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Apcotex Apcoflex® N5 High ACN Nitrile Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Apcoflex® N5 is a hot polymerized, high CAN containing acrylonitrile butadiene co-polymer. It contains non-staining antioxidant.

Applications: Apcoflex® N5 is designed to have high strength and high oil resistance because of its very high Mooney viscosity and high acrylonitrile content. The polymer has low nerve and hence has good extrusion and calendaring properties. The polymer as such and in form of blends with other compatible elastomers is suited for production of hoses, tubes, covers and belts. .The co-polymer has high MEK solubility and is specifically recommended for use in cements, adhesives, grouts, spreading applications such as printing blankets and friction material such as brake lining etc.

CAS No,: 9003-18-3

Information provided by Apcotex Industries Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.70 %<= 0.70 %
Viscosity <= 2100 cP<= 2100 cPCement
Mooney Viscosity 80 - 95
@Temperature 100 °C
80 - 95
@Temperature 212 °F
ML 1+4
Ash <= 0.75 %<= 0.75 %
Storage Temperature <= 35.0 °C<= 95.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life <= 24.0 Month<= 24.0 Month
 
Descriptive Properties
Content29-34%Bound Acrylonitrile
Solubility80-98%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAPCOT012 / 315591

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.