MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Johnson Matthey Argo-braze™ 61V Silver Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Argo-braze™ 61V is a silver-copper-indium brazing filler metal. It is manufactured only as a vacuum tube grade material with low and controlled levels of volatile impurities. The indium content of this filler metal reduces the alloy’s melting temperature and gives it improved wetting on ferrous parent metals over the straight silver-copper filler metal Argo-braze™ 72V.

Argo-braze™ 61V is intended for use in fluxless atmosphere (reducing or inert gas) or vacuum brazing applications, however, it is prone to liquate (separate into low and high melting constituents) if it is heated slowly through its melting range. For this reason rapid heating methods should be employed wherever possible.

This filler metal is typically used for brazing vacuum tube type components and for the brazing of metalized ceramics in vacuum tube devices or in the production of ceramic to metal seals. Where ceramics are being brazed to a low expansion nickel alloy care should be taken (nickel plating / stress relieving) to prevent intergranular penetration (liquid metal stress cracking) of the nickel alloy.

This filler metal was formerly called IN15.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 630 - 705 °C
Solidus 630 °C
Liquidus 705 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 24 %
Indium, In 14.5 %
Silver, Ag 61.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
Lucas-Milhaupt Lucanex 616 Active Metal Brazing
Indium Corp. Indalloy 179 Silver Solder Alloy
Johnson Matthey Argo-braze™ 502 Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 56 Silver Brazing Filler Metal

NJMMJ9711 / 186112

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.