MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger ENSIPRO® Polypropylene - Extruded Products (PP)  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: ENSIPRO (polypropylene ) is a homopolymer polyolefin engineering plastic providing excellent chemical resistance and high purity. FDA compliant with better mechanical properties than other typical polyolefin materials, it is light weight, weldable, and unaffected by moisture.

Uses: ENSIPRO's excellent chemical resistance and high purity characteristics make it ideal for use in the food-processing industries. Common applications include pump and valve components, tanks, laboratory equipment, and other parts in contact with corrosive environments.

Ensipro grades have been replaced by Tecafine

Information supplied by Ensinger, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Water Absorption 0.010 - 0.030 %0.010 - 0.030 %24 hrs.; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9090ASTM D785
Tensile Strength, Ultimate 32.2 MPa4670 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Modulus of Elasticity 0.896 GPa130 ksi1% Secant; ASTM D638
Flexural Yield Strength 41.0 - 55.0 MPa5950 - 7980 psiASTM D790
Flexural Modulus, 1% Secant 1200 MPa174000 psiASTM D790
Izod Impact, Notched 0.480 J/cm0.899 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmASTM D257
Dielectric Constant 2.2
@Frequency 60 Hz
2.2
@Frequency 60 Hz
50% RH; ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C
@Temperature 20.0 °C
50.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Melting Point 160 - 174 °C320 - 345 °F
Deflection Temperature at 1.8 MPa (264 psi) 49.0 - 60.0 °C120 - 140 °FASTM D648
Flammability, UL94 HBHB
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Addiplast Addilene H 560 Polypropylene Homopolymer
Addiplast Addilene H 462 M20 Polypropylene Homopolymer
Overview of materials for Polypropylene, Extrusion Grade
Network Polymers NPP 30-0300
Ineos H38G-02 Polypropylene Homopolymer

PENS09 / 35974

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.