MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Synesstic™ 12 Synthetic Fluid
Categories: Fluid; Lubricant; Alkylated Naphthalene (AN)

Material Notes: Product Description: Synesstic™ Alkylated Naphthalene (AN) represent a unique class of API Group V category fluids. Synesstic™ AN products offer improved hydrolytic, thermal and oxidative stability versus other Group V fluids. Synesstic™ AN products are particularly suited for use as a blendstocks in synthetic lubricant applications that require high stability under extreme operating conditions.

Appearance: Bright & Clear

Availability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South America

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.887 g/cc
@Temperature 15.6 °C
ASTM D4052
Brookfield Viscosity 22000 cP
@Temperature -15.0 °C
ASTM D2983
Viscosity Measurement 105Index; ASTM D2270
Kinematic Viscosity 392500 cSt
@Temperature -40.0 °C
ASTM D445
Kinematic Viscosity at 40°C (104°F) 109 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 12.4 cStASTM D445
Evaporation Loss 6.3 %
@Temperature 205 °C,
Time 23400 sec
ASTM D972
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.050[mg KOH/g]; ASTM D974 (mod)
 
Electrical PropertiesOriginal ValueComments
Dielectric Breakdown 50000 V
 
Thermal PropertiesOriginal ValueComments
Pour Point -33.0 °FASTM D5950/D97
Flash Point 464 °FPMCC; ASTM D92
 496 °FCOC; ASTM D92
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.506ASTM D1218
 
Component Elements PropertiesOriginal ValueComments
Bromine, Br <= 1.00 %Bromine Number; ASTM D1159 (mod)
 
Descriptive Properties
Aniline Point194°FASTM D611
Color<4.0ASTM D1500
CompositionWater<50 ppm, ASTM D6304 (mod)
Density Correction Factor0.000540 (g/cc)/°CASTM D1250
Elastomer Compatibility (%)0Fluoroelastomer Hardness Change, ASTM D471
 -0.1Fluoroelastomer Elongation Change, ASTM D471
 0.4Fluoroelastomer Volume Change, ASTM D471
 1.2Polyacrylate Volume Change, ASTM D471
 10Nitrile Volume Change, ASTM D471
 -12.7Nitrile Tensile Strength Change, ASTM D471
 15.7Polyacrylate Tensile Strength Change, ASTM D471
 2Polyacrylate Hardness Change, ASTM D471
 -21.4Nitrile Elongation Change, ASTM D471
 -24.8Polyacrylate Elongation Change, ASTM D471
 3Nitrile Hardness Change, ASTM D471
 5Fluoroelastomer Tensile Strength Change, ASTM D471
Fire Point554°FCOC, ASTM D92
Hydrolytic Stability, TAN Change0.02 mg KOH/gASTM D2619
Kauri-Butanol Value10ASTM D1133
Noack Volatility (%)4.5ASTM D5800/DIN 51581
RPVOT>1400 minWith AO, ASTM D2272
 180 minNeat, ASTM D2272

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nye Lubricants 761G Grease
Aluminum 6061A Composition Spec
ExxonMobil Synesstic™ 5 Synthetic Fluid
ExxonMobil SpectraSyn Ultra™ 150 High VI Polyalphaolefin (PAO) Fluid
Lubriplate 68-N Naphthenic Refrigeration Compressor Oil

PEX99697 / 175933

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.