MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polytek PlatSil® 73-45 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: PlatSil® 71 & 73-Series Silicone Rubbers are twocomponent, room temperature curing (RTV) systems that cure to flexible, high-strength rubbers. These platinum-cured (or additioncured) systems can be used to make flexible molds or parts that offer excellent release properties, good chemical resistance, and high dimensional stability. PlatSil® molds offer long library life and are a good choice for casting resin (polyurethane, polyester, epoxy), polyurethane rubber and foam, wax, plaster and concrete. Polytek offers additives to vary viscosity and cure time of the liquid rubber, as well as hardness and color of the cured rubber.

Product Line Features:

  • Two-part, platinum-cured (addition-cured) silicone rubbers
  • Room temperature curing (RTV)
  • Range of hardness from A10 to A60
  • Reproduces fine details
  • Low shrinkage upon cure; high dimensional stability
  • Release agents not required for casting many materials in PlatSil® molds
  • Cured molds have long library life
  • Thicken with liquid thickener for brush-on application

Information provided by Polytek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/cc
Viscosity 35000 cP35000 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4545
Tensile Strength 4.35 MPa631 psi
Elongation at Break 707 %707 %
Tear Strength 11.0 kN/m62.9 pliDie T
 25.4 kN/m145 pliDie B
 
Processing PropertiesMetricEnglishComments
Cure Time 40.0 min0.667 hourPour Time
 960 min16.0 hourDemold Time
 2880 min48.0 hourTotal Cure
 
Descriptive Properties
Cured ColorGreen
Mix Ratio By Weight1A:10B
Part A ColorGreen
Part B ColorTan
Specific Volume21.3 in3/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTK5008 / 251000

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.