BJ998MO - is a very high melt flow heterophasic copolymer with high/medium impact strength and stiffness. This grade is designed for high-speed injection molding and contains nucleating and antistatic additives. The material is nucleated with Borealis Nucleation Technology (BNT). Flow properties, nucleation and good stiffness give potential for cycle time reduction. Components molded from this grade have good demolding properties and combine good stiffness, gloss and antistatic properties with good low-temperature impact strength. Cas No. 9010-79-1 Typical characteristics: - High stiffness
- Good gloss
- High impact strength
- Excellent antistatic properties
Applications: - Caps and closures
- Thin wall containers
- Lids
- Thin wall packaging
Information provided by Borealis AG |