Low density polyethylene for injection molding Applications: - Medium sized moldings
- Lids
- Compounding
- Carpet backing
- Bottle closures
Additives: Barefoot Advantages: - High flow
- Good toughness
- Excellent gloss
- Good flexibility
Information provided by Titan Chemicals |