MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Chemlok® 481/Curative 44 Adhesive, 481 Adhesive System
Categories: Polymer; Adhesive; Thermoset

Material Notes: LORD Chemlok® 481/Curative 44 adhesive is a two-component adhesive system used to bond thermoplastic elastomers (TPEs) to metals during the injection molding process. This adhesive system can also be used to fabricate hose for cold and hot [54-65°C (130-150°F)] liquids.

Features: bonds a wide variety of thermoplastic elastomers to metal. applies easily by spray, brush or dip methods. requires only a single coat for most applications. For harsh environments, apply Chemlok 205 primer prior to adhesive application.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.35 - 7.65 lb/gal
Solids Content 17 - 20 %by weight
Viscosity Measure 400 - 1500 cSt
@Temperature 38.0 °C
 
Thermal PropertiesOriginal ValueComments
Flash Point 5.00 °CSeta
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 21.0 - 27.0 °C
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceStraw Yellow Liquid
SolventsXylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9092 / 232481

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.