MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
330 Stainless Steel
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Material Notes: The high nickel content of this electrode provides excellent resistance to heat and scale at temperatures above 1800°F, leading to uses such as heat exchangers and radiant tubes. Alloy 330 electrodes are also used for repair of defects in castings of the 330 analysis.

Key Words: UNS N08330, AMS 5592, AMS 5716, ASTM B511, ASTM B512, ASTM B535, ASTM B536, ASTM B546, SAE J405 (30330), SAE J412 (30330); RA330
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 586 MPa
 30.0 MPa
@Temperature 1150 °C
 35.0 MPa
@Temperature 1095 °C
 76.0 MPa
@Temperature 980 °C
 152 MPa
@Temperature 870 °C
 276 MPa
@Temperature 760 °C
 393 MPa
@Temperature 650 °C
 448 MPa
@Temperature 540 °C
 490 MPa
@Temperature 425 °C
 524 MPa
@Temperature 315 °C
 552 MPa
@Temperature 205 °C
Tensile Strength, Yield 290 MPa
@Strain 0.2 %
 23.0 MPa
@Strain 0.2 %,
Temperature 1150 °C
 27.0 MPa
@Strain 0.2 %,
Temperature 1095 °C
 50.0 MPa
@Strain 0.2 %,
Temperature 980 °C
 90.0 MPa
@Strain 0.2 %,
Temperature 870 °C
 138 MPa
@Strain 0.2 %,
Temperature 760 °C
 155 MPa
@Strain 0.2 %,
Temperature 650 °C
 172 MPa
@Strain 0.2 %,
Temperature 540 °C
 193 MPa
@Strain 0.2 %,
Temperature 425 °C
 217 MPa
@Strain 0.2 %,
Temperature 315 °C
 241 MPa
@Strain 0.2 %,
Temperature 205 °C
Elongation at Break 43 %in 50 mm
 22 %
@Temperature 760 °C
in 50 mm
 28 %
@Temperature 650 °C
in 50 mm
 30 %
@Temperature 870 °C
in 50 mm
 40 %
@Temperature 205 °C
in 50 mm
 53 %
@Temperature 980 °C
in 50 mm
 72 %
@Temperature 1095 °C
in 50 mm
 93 %
@Temperature 1150 °C
in 50 mm
Rupture Strength 5400 psi
@Temperature 816 °C,
Time 3.60e+6 sec
Characteristic (Heat Treatment and form unspecified)
 8500 psi
@Temperature 816 °C,
Time 360000 sec
Characteristic (Heat Treatment and form unspecified)
 10500 psi
@Temperature 732 °C,
Time 3.60e+6 sec
Characteristic (Heat Treatment and form unspecified)
 15000 psi
@Temperature 732 °C,
Time 360000 sec
Characteristic (Heat Treatment and form unspecified)
Modulus of Elasticity 197 GPa
 124 GPa
@Temperature 980 °C
 134 GPa
@Temperature 870 °C
 134 GPa
@Temperature 870 °C
 164 GPa
@Temperature 540 °C
 179 GPa
@Temperature 315 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000102 ohm-cm
@Temperature 20.0 °C
 0.000114 ohm-cm
@Temperature 425 °C
Magnetic Permeability 1.02approximate value for the annealed condition at RT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.4 µm/m-°C
@Temperature 0.000 - 100 °C
 16.0 µm/m-°C
@Temperature 0.000 - 315 °C
 16.7 µm/m-°C
@Temperature 0.000 - 540 °C
 17.3 µm/m-°C
@Temperature 0.000 - 650 °C
 18.0 µm/m-°C
@Temperature 0.000 - 870 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 12.5 W/m-K
@Temperature 24.0 °C
 16.3 W/m-K
@Temperature 100 °C
 19.4 W/m-K
@Temperature 425 °C
 21.6 W/m-K
@Temperature 500 °C
 28.5 W/m-K
@Temperature 870 °C
Melting Point 1400 - 1425 °C
Solidus 1400 °C
Liquidus 1425 °C
Maximum Service Temperature, Air 1035 °CIntermittent
 1150 °CContinuous Service
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Chromium, Cr 19 %
Iron, Fe 42 %
Manganese, Mn <= 2.0 %
Nickel, Ni 36 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.13 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
304 Stainless Steel
309 Stainless Steel
330 Stainless Steel, annealed sheet
330 Stainless Steel, annealed bar
330 Stainless Steel, annealed plate

MQ330E / 12826

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.