MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostacom ERG 393F NA BLACK Polypropylene with 20% Glass Fiber Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Hostacom ERG 393F NA BLACK is a 20% glass fiber reinforced PP copolymer, with good stiffness and impact resistance. This material provides high melt strength, good melt elongation behavior and is tailor-made for foam injection molding. The product is available in black color, pellet form. Applications: Automotive Parts, Exterior Automotive Applications, Under hood

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.0 MPa8700 psi
Tensile Modulus 5.00 GPa725 ksi
Flexural Modulus 4.20 GPa609 ksi
Charpy Impact, Notched 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostacom ERG 393F BLACK Polypropylene with 20% Glass Fiber Filler
LyondellBasell Hostacom ERG 393F C1 BLACK Polypropylene with 20% Glass Fiber Filler
LyondellBasell Hostacom ERG 393F C12509 Polypropylene with 20% Glass Fiber Filler
ExxonMobil Santoprene® 241-73W236 Thermoplastic Elastomer
Asahi Kasei Thermylene® P6-10FG-Y950 10% Glass Fiber Reinforced, Lubricated Polypropylene

PEQT7904 / 219541

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.