MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Socomore Aeroglaze® 9929 Epoxy Primer
Categories: Polymer; Thermoset; Epoxy

Material Notes: Aeroglaze® 9929 epoxy primer is designed to be used on properly prepared aluminum and steel surfaces for applications that require protection against corrosion.

Socomore acquired the Aeroglaze® and Chemglaze® product lines from Lord in September 2016.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/cc9929B; ASTM D1475-85
 1.35 g/ccMixed; ASTM D1475-85
 1.48 g/cc9929A; ASTM D1475-85
Solids Content 47.2 %9929A; by volume; ASTM D2369-87 Modified
 49.8 %Mixed; by volume; ASTM D2369-87 Modified
 58.8 %9929B; by volume; ASTM D2369-87 Modified
 61.7 %9929B; by weight; ASTM D2369-87 Modified
 68.6 %Mixed; by weight; ASTM D2369-87 Modified
 69.8 %9929A; by weight; ASTM D2369-87 Modified
Volatile Organic Compounds (VOC) Content 355 g/l9929B; ASTM D3960-89
 436 g/lMixed; ASTM D3960-89
 450 g/l9929A; ASTM D3960-89
Brookfield Viscosity 390 cP
@Temperature 25.0 °C
9929B; ASTM D2369-87; LVT
 735 cP
@Temperature 25.0 °C
Mixed; ASTM D2369-87; LVT
 4800 cP
@Temperature 25.0 °C
9929A; ASTM D2369-87; LVT
Outgassing - Total Mass Loss 1.93 %ASTM E595-77
 
Thermal PropertiesOriginal ValueComments
Flash Point 21.1 °C9929A; Setaflash, Closed Cup; ASTM D3278-82
 29.4 °C9929B; Setaflash, Closed Cup; ASTM D3278-82
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 2.00 - 4.00 hour
@Temperature 25.0 °C
1 dry mil
 7.00 - 10.0 hour
@Temperature 25.0 °C
4 dry mils
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClear Amber9929B
 YellowMixed
 Yellow9929A
Coating Film Dry Weight (gm/ft²/mil)4.81
Mix Ratio3.5:1by volume
 5.5:1by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD121 / 86129

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.