MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman MPP40FJ16BK 40% Mica Filled, Chemically-Coupled, Heat-Stabilized, Homopolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Mica Filler

Material Notes: 40% Mica Filled, Chemically-Coupled, Heat-Stabilized, Homopolymer Polypropylene

Description: Precolored black

Applications: Primary end use is for heater/AC housing doors.

Specifications: Meets/exceeds Ford Engineering Material Specification GMP.PP.098

Comments:
Thermal Oxidative Stability (150°C): >720 hrs. as per ASTM D3012; GMP.PP.017 Specification: 168 Min.
Mica Content: 40.3% as per ASTM ISO 3451/1

Material Pre-dry: Normally it is not necessary to pre-dry this material. However, if conditions dictate drying to optimize material properties and part appearance then dry in a desiccant dryer at 180°F for 2-3 hours or 160°F for >4 hours.
Manifolds: Maintain manifolds, runners and tips 10 to 20°F above the front one temperature to allow easier filling. (Gate drool is best eliminated using screw decompression rather than reducing tip temperature.)
Back Pressure (Range): 50-100 psi. Injection Speed: slow to medium. Screw Speed: medium. Injection Pressure: Adjust to just above a short shot. Injection Time: Adjust to just above a short shot. Cushion (Range): 0.2-0.5 in. Nozzle Type: Free flowing/Standard.
Some conditions may have to be altered to obtain acceptable parts. Please do not run too cold, molded in stress and rough surface may become a problem. If you must run below melt or temperatures recommended for dimensional precision you may compromise impact and esthetics. Retest parts to confirm performance.

Data provided by Ferro Corporation - Specialty Plastics Group.

A. Schulman has acquired the Ferro specialty plastics business.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccISO 1183 A
Linear Mold Shrinkage 0.010 - 0.013 cm/cmISO 2577
Melt Flow 10.5 g/10 minISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 32.2 MPaISO 527
Flexural Modulus 4.179 GPaISO 178
Izod Impact, Notched (ISO) 2.40 kJ/m²ISO 180/1A
 1.90 kJ/m²
@Temperature -40.0 °C
ISO 180/A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 137 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °CISO 75
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 400 - 415 °F
Middle Barrel Temperature 410 - 425 °F
Front Barrel Temperature 420 - 435 °F
Nozzle Temperature 425 - 440 °F
Mold Temperature 100 - 115 °FCore. Cooler temperatures may be needed to maintain dimensions or eliminate sinks in thick sections.
 110 - 135 °FCavity
Drying Temperature 180 °F2-3 hrs at 180°F or 4+ hours at 160°F.
Dry Time 2 - 3 hour
 
Descriptive Properties
ColorPrecolored black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Washington Penn High Modulus Polypropylene Homopolymer 40% Mica Filled
Washington Penn High Modulus Polypropylene Homopolymer 40% Glass Filled
Washington Penn Homopolymer Polypropylene 40% Glass Reinforced
Washington Penn PPH3TF4-BLK Polypropylene, 40% Talc Filled
A. Schulman TPP40AC52BK 40% Talc Filled, Heat Stabilized, Homopolymer Polypropylene

PFERRO22 / 38136

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.