MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Fluorseals PTFE 25% glass filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: Improved compressive strength and wear resistance.

Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.24 g/cc0.0809 lb/in³ASTM 1457-62 T
Deformation 7.0 - 14 %7.0 - 14 %14 MPa, 100 h, 23°C; ASTM D621-59
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 30.0 MPa4350 psiASTM 1457-62 T
Tensile Strength at Break 15.0 MPa2180 psiASTM 1457-62 T
Elongation at Break 370 %370 %ASTM 1457-62 T
Coefficient of Friction, Dynamic 0.145 - 0.170.145 - 0.17v = 1 m/s
 0.14 - 0.210.14 - 0.21v = 1.9 m/s
Abrasion 2.12.1mm of depth after 200 hrs load duration; Partner Material ST 50
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmDIN 53482
Surface Resistance 1.00e+16 ohm1.00e+16 ohmDIN 53482
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 µm/m-°C
@Temperature 100 °C
55.6 µin/in-°F
@Temperature 212 °F
DIN 52328
Thermal Conductivity 0.350 W/m-K2.43 BTU-in/hr-ft²-°FDIN 52612

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Isoflon PTFE + 25% Glass Polytetrafluoroethylene with 25% Glass
Fluorseals PTFE 60% bronze filled
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled
Quantum PEEK 30% Carbon Filled
Dalau Dalcon 086 100% Virgin PTFE modified polymer

PTEKU2 / 70055

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.