MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger NORYL® Polyphenylene oxide (PPO)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes: NORYL®, due to its inherent chemical composition, exhibits unusually low moisture absorption. Therefore, good electrical insulating properties are realized over a wide range of humidity and temperature conditions. Chemical attack from water, most salt solution, acids and bases is also minimal with NORYL®. The addition of glass fiber reinforcement enhances both the mechanical and thermal properties of the basic NORYL® material.

  • Good electrical insulating properties (Due to its extremely low water absorption with values as low as 0.07%, NORYL® is an excellent electrcial insulating material
  • Long-term dimensional stability
  • Superior impact strength (NORYL® exhibits a continuous use temperature in excess of 220°
  • Wide ranger of UL flammability ratings from UL94 HB to UL94 V-1
  • FDA compliance for certain grades
  • Light weight (NORYL®, with a density of 0.0383 lbs/in3, can be used in applications where weight is a significant consideration)
  • Thermoformable capability
  • Possesses good hydrolytic stability

Information Provided by Ensinger Industries, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Density 0.0383 lb/in³ASTM D792
Water Absorption 0.070 %
@Temperature 22.8 °C,
Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 119ASTM D785
Tensile Strength at Break 9200 psi
@Temperature 22.8 °C
ASTM D638
Elongation at Break 25 %
@Temperature 22.8 °C
ASTM D638
Tensile Modulus 350000 psi
@Temperature 22.8 °C
ASTM D638
Flexural Strength 13400 psi
@Temperature 22.8 °C
ASTM D790
Flexural Modulus 370000 psi
@Temperature 22.8 °C
ASTM D790
Izod Impact, Notched 3.50 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Coefficient of Friction, Dynamic 0.39
@Pressure 0.276 MPa
50 fpm
Coefficient of Friction, Static 0.32
@Pressure 0.276 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cm
@Temperature 22.8 °C
ASTM D257
Dielectric Constant 2.7
@Frequency 60 Hz,
Temperature 22.8 °C
50% RH; ASTM D150
Dielectric Strength 500 V/milASTM D149
Dissipation Factor 0.00070
@Frequency 60 Hz,
Temperature 22.8 °C
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 33.0 µin/in-°F
@Temperature -17.8 - 60.0 °C
ASTM D696
Maximum Service Temperature, Air 220 °FLong Term
 230 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 279 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 254 °FASTM D648
Vicat Softening Point 310 °F
Flammability, UL94 V-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
GEHR Plastics Noryl PPO
Omnia Plastica Noryl® PPO m Polyphenylenoxide
Overview of materials for Acetal Homopolymer, PTFE-Filled
GEHR Plastics Noryl PPO-30 GF 30% Glass Filled
Overview of materials for Polyetheretherketone, Unreinforced

PENSIN007 / 92824

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.