MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik Osprey 4140/MA Low Alloy Steel Master Alloy Powder (Grade 80% - 22)
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: Particle size distribution 1-250 microns. Typical distribution:
  • 80% < 22 microns
  • 67% < 16 microns
  • 43% < 10 microns
  • 14% < 5 microns
Mean size is 12 microns.

Master alloy blended with 2 parts iron to produce 4140MA alloy after sintering. SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requirements.

The specifications listed are subject to the benefits and scrutiny of Osprey's accreditation to ISO 9001.

Information provided to MatWeb by Osprey Metals, now Sandvik Osprey Ltd.

Key Words: UNS G41400; medium-carbon steels, medium carbon steels, alloy steels, Powder metallurgy, master alloy, Metal Powder, Metal Injection Molding, MIM, Microfine
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 12 µmMean
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.14 - 1.29 %
Chromium, Cr 2.4 - 3.3 %
Iron, Fe 91.9 %As Balance
Manganese, Mn 2.25 - 3.0 %
Molybdenum, Mo 0.45 - 0.75 %
Phosphorus, P <= 0.035 %
Silicon, Si 0.45 - 1.05 %
Sulfur, S <= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
AISI 4140 Steel, normalized at 870°C (1600°F), air cooled, 13 mm (0.5 in.) round
AISI 4140 Steel, oil quenched, 13 mm (0.5 in.) round [845°C (1550°F) quench, 540°C (1000°F) temper]
AISI 4140 Steel, oil quenched, 540°C (1000°F) temper, 25 mm (1 in.) round
Crucible Steel MAXEL® Tooling Alloy Steel, AISI 4140 Modified

NOSPR048 / 18570

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.