MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Moplen HP648T Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Moplen HP648T is a homopolymer used in injection molding. This grade is characterized by a high flow, medium stiffness combined with a Nucleation and an antistatic activation. Moplen HP648T is typically used in house ware, TWIM food and Non-food containers.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183-1
Melt Flow 53 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 35.0 MPaISO 527-1,-2
Elongation at Break >= 50 %ISO 527-1,-2
Elongation at Yield 8.0 %ISO 527-1,-2
Tensile Modulus 1600 MPaISO 527-1,-2
Charpy Impact, Notched 2.00 kJ/m²
@Temperature 23.0 °C
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 154 °CA50; ISO 306
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Moplen HP648H Polypropylene
BASF Novolen® 1148 TC Polypropylene
Borealis Borecene™ RM8342RC Linear Polyethylene for Rotational Molding
Borealis BorPEX™ HE2515 High Density Polyethylene Compound for Silane Crosslinked Pipes
Borealis BorPURE™ RE450MO Polypropylene Random Copolymer

PEQT9070 / 220701

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.