MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Osterman & Co Osterlene® PPC20-2NA Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Product Description: PPC20-2NA is a medium impact polypropylene copolymer formulated for injection molding applications requiring a balance of medium impact resistance, stiffness and high-flow. PPC20-2NA contains an anti-static and nucleating agent

Availability: North America
Additive: Antistatic; Nucleating Agent
Features: Antistatic; High Flow; High Stiffness; Impact Copolymer; Medium Impact Resistance; Nucleated
Processing Method: Injection Molding

Information provided by Osterman & Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9292ASTM D785
Tensile Strength, Yield 26.1 MPa3780 psiASTM D638
Elongation at Yield 4.0 %4.0 %ASTM D638
1% Secant Modulus 1310 MPa190000 psiFlexural; ASTM D790
Izod Impact, Notched 1.07 J/cm2.00 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 42.0 kJ/m²20.0 ft-lb/in²ASTM 4812
Gardner Impact 20.3 J
@Temperature -17.8 °C
15.0 ft-lb
@Temperature 0.000 °F
ASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C219 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POSTER144 / 267726

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.