MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tisan TISARBON® Flame Retardant (V0) Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products industries. General Specifications include:
  • High temperature resistance
  • Dimensional stability
  • Impact resistance
  • Excellent surface quality
  • High light transparence
  • Flame resistance
  • Low moisture ratio
  • Toughness
TISARBON has good chemical resistance against weak acids. It has medium resistance against alcohols, hydrocarbons, and engine fuels, and weak resistance against acids, alkalis, and organic solvents.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Moisture Absorption 0.20 %ISO 62
Linear Mold Shrinkage 0.0050 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPaISO 527-2
Tensile Strength, Yield 60.0 MPaISO 527-2
Elongation at Break 6.5 %ISO 527-2
Elongation at Yield 5.0 %ISO 527-2
Modulus of Elasticity 2.30 GPaISO 527-2
Izod Impact, Notched (ISO) 10.0 kJ/m²ISO 180
 
Thermal PropertiesOriginal ValueComments
Melting Point 230 °C
Vicat Softening Point 141 °CISO 306
Heat Distortion Temperature 135 °CISO 75-2
Flammability, UL94 V-0
Glow Wire Test 960 °C60695-2-10
 
Processing PropertiesOriginal ValueComments
Feed Temperature 70.0 °C
Rear Barrel Temperature 280 - 290 °CAft-1. Region Temperature
Middle Barrel Temperature 270 - 280 °CMid-2. Region Temperature
Front Barrel Temperature 260 - 270 °CPre-3. Region Temperature
Nozzle Temperature 280 - 290 °C
Melt Temperature 270 - 290 °C
Drying Temperature 90.0 - 120 °CPredrying Temperature
Dry Time 3 - 5 hourPredrying Time
 
Descriptive Properties
Block Temperature80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tisan TISLAMID® 6 UNR Nylon 6
Tisan TISARBON® 10% Glass Fiber Reinforced Polycarbonate
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
Overview of materials for Polycarbonate, 20% Glass Filled
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled

PTIS068 / 79503

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.