MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Rohacell® P 190 Polymethacrylimide (PMI) Rigid Foam Sheet  (discontinued **)
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polymethacrylimide

Material Notes: ROHACELL P 190 is a compacted grade with an oriented cell structure leading to high strength and rigidity in the plane of the sheet.

General ROHACELL Information: ROHACELL is a closed-cell rigid expanded plastic material for lightweight sandwich construction. It has excellent mechanical properties, high dimensional stability under heat, solvent resistance and, particularly at low temperature, a low thermal conductivity. The strength and moduli values are the highest are the highest for any foamed plastic in its density range. ROHACELL is manufactured by hot forming of methacrylic acid/methacrylonitrile copolymer sheets. During foaming this copolymer is converted to polymethacrylimide.

Information supplied by Emkay Plastics, Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 11.9 lb/ft³ASTM D1622-63
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1210 psiASTM D638-68
Elongation at Break 6.0 %ASTM D638-68
Modulus of Elasticity 54.0 ksiASTM D638-68
Flexural Yield Strength 1710 psiPerpendicular to Sheet; ASTM D 790-66
 1780 psiASTM D790-66
Compressive Yield Strength 455 psiPerpendicular to Sheet; ASTM D 1621-64
 1110 psiASTM D1621-64
Shear Modulus 14.2 ksiASTM C273-61
Shear Strength 427 psiPerpendicular to Sheet; ASTM C 273-61
 782 psiASTM C273-61
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °CDimensional stability per DIN 53424; oriented cell structure starts to decrease beyond this temperature.
 
Descriptive Properties
ColorWhite

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Rohacell® P 170 Polymethacrylimide (PMI) Rigid Foam Sheet
Hexcel® HexForce™ 1168 Hybrid Composite Fabric
Hexcel® HexForce™ 1035 Fiber Glass Fabric
Evonik Rohacell® 71 IG-F Industrial Grade Polymethacrylimide (PMI) Foam
Evonik Rohacell® 70 Polymethacrylimide (PMI) Rigid Foam Sheet

PROHA05 / 66310

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.