MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Matexcel MoS-031 ZSM-5 Molecular Sieve
Categories: Other Engineering Material

Material Notes: ZSM-5 molecular sieves have been widely used in petrochemical, coal chemical and fine chemical fields, such as catalytic cracking, diesel pour point depressurization, catalytic dewaxing, shape-selective catalysis, aromatization of straight-run gasoline to improve octane number, toluene isomerization, xylene isomerization, methanol conversion to gasoline, methanol dehydration to dimethyl ether, aromatization of low-carbon hydrocarbons, C3-C4 fraction superposition to gasoline, etc.

Morphology: Powder

Key Words: Synonyms: ZSM-5 Molecular Sieve
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Product overviewPore size (nm): 0.53~0.58 Si/Al ratio:>45 BET specific surface area (m2/g): =310 Relative crystallinity (%): =95 Residual sodium (%): =0.1 Burn reduction (%): =5 Particle size (um): 3~5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMXCK2050 / 300681

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.