MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 4099X67316C Polyphthalamide, GF, Stainless Steel Fiber, EMI  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), Stainless Fiber Filled/EMI

Material Notes: Data is for injection molded specimens and was provided by the manufacturer, RTP Company.

This product has been discontinued, please contact RTP Company regarding alternate grades.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.64 g/ccASTM D792
Water Absorption 0.20 %24 hrs @ 23°C; ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm
@Thickness 6.40 mm
ASTM D955
 0.0040 cm/cm
@Thickness 3.20 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.016 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 138 MPaASTM D638
Elongation at Break 1.5 %ASTM D638
Tensile Modulus 10.3 GPaASTM D638
Flexural Yield Strength 241 MPaASTM D790
Flexural Modulus 10.3 GPaASTM D790
Izod Impact, Notched 0.500 J/cm
@Thickness 3.20 mm
ASTM D256
Izod Impact, Unnotched 4.80 J/cm
@Thickness 3.20 mm
ASTM D256
K (wear) Factor 5000 x 10-10 in³-min/ft-lb-hrat 50 fpm, 2000 PV against C1018 Steel HRC 15-25, 14-17 microsmoothness; ASTM D 3702
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.200 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 266 °CASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
HB; UL94. Values per RTP Company Testing.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 283 D TFE 15 Nylon 6/12 (PA), Carbon Fiber - PTFE Lubricated
RTP Company RTP 2799S X 89622 C  Styrenic Thermoplastic Elastomer (TES) Thermally Conductive - Electrically Conductive - SEBS
RTP Company RTP 285 D SI 2 Nylon 6/12 (PA), Carbon Fiber - Silicone Lubricated
Eurotec® Tecomid® NT40 GR15 NL HS PPA, 15% glass fiber reinforced, heat stabilized, natural
RTP Company RTP 2799 S X 91655 BLACK Saturated Styrenic Block Copolymer

PRRY95 / 66477

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.