MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Versalis Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Product Description:
  • Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of blowing agent. Extir CM does not contain CFC or HCFC. Extir CM Giotto 5 is a white product with improved thermal conductivity.

    Applications: Extir CM Giotto 5 has an improved coefficient of thermal insulation. Blocks exhibit good compressive strength and fusion combined with an excellent surface finish after cutting. Typical applications are:

    • low density blocks for thermal insulation
    • composite EPS/plasterboard for internal wall insulation
    • low density flooring slabs
    • cut packaging

    Information provided by Polimeri Europa.

    Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.590 - 0.630 g/cc
Density >= 0.0120 g/ccMinimum apparent density on a continuous pre-expander after two expansions
 >= 0.0160 g/ccMinimum apparent density on a discontinuous pre-expander
 >= 0.0180 g/ccMinimum apparent density on a continuous pre-expander after one expansion
 0.0120 - 0.0250 g/ccDensity range normally used
Particle Size 900 - 1600 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Extir® LN 2000 Expandable Polystyrene
BASF Styropor® P 240 EPS
BASF Styropor® P 340 EPS
BASF Styropor® P 440 EPS
Versalis Extir® CM Galileo Europa 5 Expandable Polystyrene - Continuous Mass

PENG163 / 124557

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.