MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical HI835H PMMA, Impact Resistant Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded

Material Notes: Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materials

Features:

  • Excellent transparency and elegance
  • Weather resistance and chemical resistance
  • Surface hardness and coloring property
  • Superior electrical resistance and mechanical properties
  • No harm caused

Applications:

  • Automotive Parts:
    • Rear lamp cover
    • Turn signal lamp cover
    • Indoor lamp cover
    • Rear quarter glass
    • Automotive badge
  • Electric or Electronic Parts:
    • LCD light guide plate
    • Microwave oven door/front panel
    • Cassette door
    • VCR cover/front panel
    • Car stereo panel
    • Dial scale
    • Light pipe
  • Sheet:
    • Signboard
    • Showcase
    • Light dome
    • Aquarium
    • Picture frame
  • Lighting and Miscellaneous:
    • Solid surface
    • Lighting cover
    • Ornaments
    • Watch crystal
    • Optical lens
    • Piano keyboard

Information Provided by LG Chem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccASTM D792
Water Absorption 0.40 %24 hours; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cmASTM D955
Melt Index of Compound 1.8 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 47ASTM D785
Tensile Strength at Break 40.0 MPaASTM D638
Elongation at Break 90 %ASTM D638
Flexural Strength 72.0 MPaASTM D790
Flexural Modulus 1.824 GPaASTM D790
Izod Impact, Notched 53.0 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.5
@Frequency 60 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm4kV/s; ASTM D149
Dissipation Factor 0.040
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °CASTM D648
Vicat Softening Point 97.0 °C1 kg; ASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ASTM D542
Haze 1.0 %
@Thickness 3.20 mm
ASTM D1003
Transmission, Visible 91 %
@Thickness 3.20 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 210 - 250 °CInjection molding cylinder temperature
Mold Temperature 60.0 - 70.0 °C
Drying Temperature 60.0 - 70.0 °C
Dry Time 4 - 6 hour
Injection Pressure 49.0 - 108 MPa
Annealing Temperature 60.0 - 70.0 °C3-5 hours

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical HI835M PMMA, Impact Resistant Grade
LG Chemical HI835S PMMA, Impact Resistant Grade
LG Chemical HI835HS PMMA, Impact Resistant Grade
LG Chemical HI855H PMMA, Impact Resistant Grade
LG Chemical HI855HS PMMA, Impact Resistant Grade

PLGCHEM249 / 51070

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.