MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling SUSTAMID® 6G PLUS PA 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Product characteristics:
  • Very good stiffness
  • Low deformation under pressure load
  • Good wear resistance
Product applications:
  • Mechanical engineering
  • Steel industry
  • Electrical industry

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccDIN EN ISO 1183-1
Water Absorption 2.0 %DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82DIN EN ISO 868
Tensile Strength, Yield 76.0 MPaDIN EN ISO 527
Elongation at Break 7.0 %DIN EN ISO 527
Modulus of Elasticity 4.00 GPaDIN EN ISO 527
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°CDIN 53752
Specific Heat Capacity 1.70 J/g-°CDIN 52612
Thermal Conductivity 0.270 W/m-KDIN 52612-1
Melting Point 218 °CISO 11357-3
Maximum Service Temperature, Air 110 °Clong term
 170 °Cshort term
Deflection Temperature at 1.8 MPa (264 psi) 100 °CDIN EN ISO 75
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 HB
@Thickness 3.00 mm
 V-2
@Thickness 6.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PROCH9313 / 233015

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.