MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Copper, UNS C43500, H02 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability for forming and bending.

Applications: bourdon tubing and musical instruments.

Test specimen: flat products - 1mm thickness.

Key Words: ISO CuZn19Sn, CEN CW701R, 205 brass
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.66 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 72
Tensile Strength, Ultimate 450 MPa
Tensile Strength, Yield 370 MPa
@Strain 0.5 %
Elongation at Break 16 %In 50 mm
Modulus of Elasticity 110 GPa
Poissons Ratio 0.38calculated
Machinability 30 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 40.0 GPa
Shear Strength 286 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000620 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.4 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.380 J/g-°C
Melting Point 965 - 1005 °C
Solidus 965 °C
Liquidus 1005 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 79 - 83 %
Iron, Fe <= 0.050 %
Lead, Pb <= 0.10 %
Other, total <= 0.15 %
Tin, Sn 0.60 - 1.2 %
Zinc, Zn 18.1 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
365.0 Aluminum Composition Spec
Copper, UNS C41500, H03 Temper flat products
Copper, UNS C40800, H08 Temper flat products
Copper, UNS C27000 (Yellow brass), H02 Temper wire
Copper, UNS C26800 (Yellow brass), OSO15 Temper flat products

MC43500b4 / 11358

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.