MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SunChemical Gwent C2010517D4 Carbon/Graphite Ink  (discontinued **)
Categories: Fluid; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Carbon Graphite Ink C2010517D4 is designed to be used for screen printing working electrodes. This is a carbon graphite ink which has been optimized to give superior electrochemical performance coupled with high speed printing. It combines good line definition and good electrochemical performance, where chromoamperometry is employed.

The ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles. It is a Polymer System for printing on polyester, PVC, Polycarbonate etc and on alumina.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 5500 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
Haake VT 550 PK1.1°
Thickness 10.0 micronsprinted through a 230 mesh SS screen with 13 micron emulsion back off
Storage Temperature 20.0 °C
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 80 ohmcured film; 11 microns thick
 
Processing PropertiesOriginal ValueComments
Cure Time 0.167 hour
@Temperature 80.0 °C
 0.500 hour
@Temperature 60.0 °C
Shelf Life 3.00 Month
 
Descriptive Properties
Coverage cm2/g700230 mesh polyester mesh screen with 13 micron emulsion back off
Printing Mesh counts/inch150 to 250stainless steel or polyester screens

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALTECH® PA66 A 1000/517.01 IM Nylon 66
Tra-Con Tra-Bond 2170T Flexible Plastic Bonder
Toagosei America Aron Alpha® Industrial Krazy Glue™ 101 Cyanoacrylate Adhesive
Taiwan Sheen Soon Sheenthane® AS-626SL TPU for PU Adhesive
Taiwan Sheen Soon Sheenthane® AH-701 TPU for Hotmelt Adhesive

WGEM053 / 75906

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.