Description: Hifax™ HSBMCB1158LS high melt flow, 1,200 MPa flexural modulus, mineral filled thermoplastic elastomeric olefin (TEO) resin has a unique balance of flow, rigidity, low temperature impact resistance, dimensional stability and paintability. It was designed for thin-walled bumper fascia applications that require high paint durability. Features include: high flow, high stiffness, excellent impact resistance, good mold filling capability, good dimensional stability, and very good paint durability. Typical applications include painted automotive thin-walled bumper fascias. Uses: Fascias Information provided by Basell. |