MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Barlog Plastics KEBATER B610 PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled

Material Notes: PBT unreinforced, high viscosity, injection molding grade with optimized toughness

Properties: dimensionally stable, good chemical resistance, Good electrical properties, good gliding properties, good aging behavior, High wear resistance, semi-crystalline

Typical areas of application: Controls, Fasteners, Actuating elements, Cover, Housing, Handles, industrial goods, Sports & Leisure Articles, shockproof housing, Structural components, Connecting elements

Industries: Automotive, Household appliances, Industry, Agriculture, Mechanical Engineering, Sports & Recreation

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ISO 1183-1
Moisture Absorption 0.100 %0.100 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0160 cm/cm0.0160 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0170 cm/cm0.0170 in/inISO 294-4
Melt Flow 10.0 g/10 min
@Load 2.16 kg,
Temperature 235 °C
10.0 g/10 min
@Load 4.76 lb,
Temperature 455 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 53.0 MPa7690 psiISO 527-1
Elongation at Break 25.0 %25.0 %ISO 527-1
Modulus of Elasticity 2.50 GPa363 ksiISO 527-1
Charpy Impact Unnotched  10.0 J/cm²
@Temperature -30.0 °C
47.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched 0.650 J/cm²3.09 ft-lb/in²ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmContact; IEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 155 °C311 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75-1/-2
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 245 - 260 °C473 - 500 °F
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 100 - 120 °C212 - 248 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.0200 %<= 0.0200 %
Back Pressure <= 4.00 MPa<= 580 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO696 / 326770

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.