MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Pearlthane® ECO D20N55D Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyurethane, TP

Material Notes: PEARLTHANE® ECO D20N55D is a 55 Shore D, High Performance natural TPU based on Renewable Sources with ca. 35% renewable content according to ASTM D6866 for Extrusion and Injection Molding applications. This natural TPU resin features properties similar to standard TPU of same hardness, i.e. excellent mechanical properties and abrasion resistance.

Applications: Pearlthane® ECO D20N55D enhances the performance of a wide range of end use products that ranges from extrusion profiles, belts, consumer electronics and sport and leisure applications, among others, where environmentally-friendly materials can bring value to the end product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D-792
Moisture Absorption at Equilibrium <= 0.10 %MQSA 44
Melt Flow 10 g/10 min
@Load 21.6 kg,
Temperature 195 - 205 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55ASTM D-2240
Tensile Strength 5520 psiASTM D-412
Tensile Stress at Strain 494.0 psi
@Strain 300 %
ASTM D-412
 2905 psi
@Strain 100 %
ASTM D-412
Elongation at Break 350 %ASTM D-412
Tear Strength 915 pliDIN 53.515
 
Thermal PropertiesOriginal ValueComments
Melting Point 383 - 401 °FTemperature range at which MFI = 10 g/10 min at 21.6 kg.; MQSA 111
Glass Transition Temp, Tg -22.0 °FDSC, 10°C/min; DIN 51.007
 
Processing PropertiesOriginal ValueComments
Feed Temperature 392 °F
Nozzle Temperature 410 °F
Mold Temperature 95.0 °F
Drying Temperature 100 - 110 °C
@Time 3600 - 7200 sec
Use of a hot air circulatory, vacuum or desiccant-air dryer is recommended.
 
Descriptive Properties
Biobased Content (%)35
Compression Zone Temperature401°F
Metering Zone Temperature410°F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMEQU973 / 109210

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.