MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Healthcare HP2REU PC (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN HP2REU is a high flow polycarbonate (PC) with an MVR (300°C/1.2kg) of 21. This is a biocompatible (ISO10993 or USP Class VI) grade for medical devices and pharmaceutical applications. It is EtO and steam sterilizable, contains mold release and adheres to our healthcare management of change policy. Available in Europe only.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.20 g/ccISO 1183
Water Absorption 0.35 %23°C/sat; ISO 62
Moisture Absorption 0.150 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 21 g/10 min
@Load 1.20 kg,
Temperature 300 °C
cm³/10 min; ISO 1133
 22 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 95.0 MPaISO 2039-1
Tensile Strength at Break 65.0 MPa50 mm/min; ISO 527
 70.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 63.0 MPa50 mm/min; ISO 527
 63.0 MPa50 mm/min; ASTM D638
Elongation at Break 100 %50 mm/min; ISO 527
 125 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %50 mm/min; ISO 527
 7.0 %50 mm/min; ASTM D638
Tensile Modulus 2350 MPa1mm/min; ISO 527
 2400 MPa5 mm/min; ASTM D638
Flexural Yield Strength 90.0 MPa2 mm/min; ISO 178
 98.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2300 MPa2 mm/min; ISO 178
 2350 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 70.0 J/mASTM D256
 30.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 65.0 kJ/m²80*10*3; ISO 180/1A
 11.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 35.0 kJ/m²ISO 179/2C
 65.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 12.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 633 JASTM D3763
Taber Abrasion, mg/1000 Cycles 10CS-17, 1 kg; SABIC method
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.7
@Frequency 50.0 - 60.0 Hz
IEC 60250
 2.7
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
Dissipation Factor 0.0010
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Thermal Conductivity 0.200 W/m-KISO 8302
Hot Ball Pressure Test 125 °CIEC 60695-10-2
 140 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 133 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 122 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 129 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 139 °CRate B/50; ASTM D1525
 140 °CRate B/50; ISO 306
 141 °CRate B/120; ISO 306
UL RTI, Electrical 130 °CUL 746B
UL RTI, Mechanical with Impact 125 °CUL 746B
UL RTI, Mechanical without Impact 125 °CUL 746B
Flammability, UL94 HB
@Thickness 3.00 mm
UL 94
 HB
@Thickness 1.50 mm
UL 94
Oxygen Index 25 %ISO 4589
Glow Wire Test 850 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ISO 489
Haze <= 0.80 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible 88 %
@Thickness 2.54 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 270 - 290 °CInjection Molding
Zone 1 260 - 280 °C
Zone 2 270 - 290 °C
Zone 3 280 - 300 °C
Melt Temperature 280 - 300 °C
Mold Temperature 80.0 - 100 °C
Drying Temperature 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10673 / 244140

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.