Notes: This compound is intended for use in medical and healthcare applications, particularly for extruded medical tubing. In addition, this grade exhibits superior dimensional stability after autoclave sterilization. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Autoclave Sterilizable; Ethylene Oxide Sterilizable; Good Processability; High Purity; Kink Resistant; No Animal Derived Components; Radiation (Gamma) Resistant Uses: Medical/Healthcare Applications; Pharmaceuticals Agency Ratings: ISO 10993 Part 5; ISO 13485 RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion Preliminary data. Information provided by Teknor Apex |