MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Applied Nanotech Ag-iJ10 Silver Ink
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Our silver nanoparticle ink technology achieves high conductivity in various formulations due to the small particle size and uniform dispersions of our inks. The low processing temperatures (70-200°C) allow for applications in printed electronics using low cost flexible polymer substrates such as PET. The small size of the nanoparticles in Ag-iJ10 make the ink suitable for printing using inkjet technologies. The solid content loading can be adjusted from 10-70 wt% to suit customer specifications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 10 - 70 %
Particle Size 0.060 µm
Viscosity 3.0 - 12 cP
Surface Tension 28 - 35 dynes/cm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.0000030 - 0.00015 ohm-cm
 
Descriptive Properties
Conductive Filler TypeSilver (Ag)
Material TypeReady-To-Use Formulation
Recommended Substratespolymer substrates such as PET
Solvent SystemOrganic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Intex® 2740 Styrene - Butadiene Copolymer
Wacker Vinnapas® LL 8251 Vinyl Acetate
BASF Ultraform® N2640 Z2 POM + PUR
BASF Master Builders Solutions ChemRex® CX Concrete Floor Primer - Epoxy
Avient Gravi-Tech™ GRV-UR-110-W Polyurethane, PUR

PFLEXCM66 / 179468

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.