MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
General Plastics LAST-A-FOAM® FP-5018 Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: FP8000 Energy Absorption Semi-rigid Series: These open-cell polyurethane foams exhibit high hysteresis (approximately 80%) as well as excellent recovery from dynamic impacts. They are available in a density range of 6 to 30 lbs. per cubic foot, and all are flame-resistant. FP8000 foam is somewhat strain-rate sensitive. Creep under high static stress is not as good as LASTAFOAM ® TF5070, TF6070 or EF4000 series foams, and this material is not recommended for constant loading. However, the outstanding hysteresis combined with quick recovery make FP8000 flexible products especially suitable for lateral (nonbearing) shock isolation. The FP8015 (15pound) density foam has served as the lateral shock-isolation system for the Peacekeeper (MX) Missile. These flame-resistant foams are also used for aircraft interior crash padding. Their low resilience allows the foam to absorb most impact energy, thus minimizing rebound and reducing injuries. These products are available as sheets, blocks and molded parts.

Advantages:

  • Absorbs significant impact energy
  • Exhibits approximately 80% hysteresis
  • Offers superb recovery from dynamic impact
  • Flame- resistant
Applications
  • Lateral (nonbearing) shock isolation
  • Aircraft interior crash padding

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.240 g/ccASTM D3574
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 133 psiASTM D3574
Tensile Modulus 689 psiASTM D3574
Flexural Strength 43.0 psiRise Parallel to Beam Thick.; ASTM D790
Flexural Modulus 931 psiRise Parallel to Beam Thick.; ASTM D790
Compressive Strength 18.0 psi
@Strain 25 %,
Temperature 65.6 °C
ASTM D1621
 69.0 psi
@Strain 25 %,
Temperature 23.9 °C
ASTM D1621
 175 psi
@Strain 50 %,
Temperature 23.9 °C
ASTM D3574
Shear Modulus 0.421 ksiRise Parallel to Specimen Width; ASTM C273
 0.447 ksiRise Parallel to Specimen Thick.; ASTM C273
Shear Strength 0.117 ksiRise Parallel to Specimen Width; ASTM C273
 0.134 ksiRise Parallel to Specimen Thick.; ASTM C273
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 109 °F
 
Descriptive Properties
Dynamic Load Deflection<129.3 gAcceleration
 279.5 in-lbsRebound (Resilience) Energy
 2820.3 in-lbsImpact Energy

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® FR-7108 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3840 FST Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3830 FST Polyurethane Foam
ExxonMobil 639 Mobil SHC 600 Series
Covestro Bayfit® SA513 Flexible Polyurethane Foam, 95 Index

PGENR083 / 186869

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.