MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ FARADEX™ Compound AS003 Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: LNP FARADEX AS003 compound is based on Acrylonitrile Butadiene Styrene (ABS) resin containing 15% stainless steel fiber. Added features of this grade include: Electrically Conductive, EMI/RFI shielding.

Features: EMI/RFI Shielding,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183
 1.16 g/ccASTM D792
Moisture Absorption 0.0500 - 0.100 %Injection Molding
 0.200 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0027 cm/cm24hrs; ISO 294
 0.0030 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0039 cm/cm24hrs; ISO 294
 0.0040 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 37.0 MPaISO 527
 39.0 MPaASTM D638
Tensile Strength, Yield 38.0 MPaISO 527
 42.0 MPaASTM D638
Elongation at Break 2.8 %ISO 527
 6.2 %ASTM D638
Elongation at Yield 2.2 %ISO 527
 2.6 %ASTM D638
Tensile Modulus 2700 MPa1 mm/min; ISO 527
 3150 MPa5 mm/min; ASTM D638
Flexural Strength 66.0 MPaISO 178
 75.0 MPaASTM D790
Flexural Modulus 2800 MPaISO 178
 3040 MPaASTM D790
Izod Impact Notched 53.0 JASTM D256
Izod Impact, Unnotched 307 J/mASTM D4812
Izod Impact, Notched (ISO) 7.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 18.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 15.0 Jpeak; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 10000 ohm-cmASTM D257
Surface Resistance 10 - 1000 ohmASTM D257
Static Decay <= 0.010 sec5000V to <50V; FTMS101B
Shielding Effectiveness 50 - 65 dB
@Thickness 3.00 mm
SABIC method
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 63.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 71.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 77.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 93.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 96.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 88.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 230 - 245 °C
Zone 3 255 - 265 °C
Melt Temperature 240 - 255 °CInjection Molding
Mold Temperature 70.0 - 95.0 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80623 / 288570

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.