MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt POLYCOR® 943 Series ISO/NPG Gel Coat
Categories: Polymer; Thermoset

Material Notes: POLYCOR® 943 Series products are high performance gel coats formulated for use in sanitary and marine applications or any FRP application where resistance to water and blistering are needed. Use of POLYCOR® 943 gel coats has enabled customers to meet and surpass all requirements of the American National Standard for plastic bath tubs, shower receptors and shower stalls, ANSI Z124.1, .2 and .3 1995, Sec. 6.1.1. These gel coats are ready to use, easy to spray, sag resistant, fast curing and require only the addition of the proper amount of an appropriate methyl ethyl ketone peroxide to cure. POLYCOR® 943 gel coats are available in whites and a wide range of colors.

Features and Benefits:

  • Resistant to water and osmotic blistering
  • Chemical resistance for a durable, long lasting finish

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 9000 - 14000 cP9000 - 14000 cPColors, RVF, spindle #4 @ 4 rpm
 16000 - 19500 cP16000 - 19500 cPWhite and Off-Whites, RVF, spindle #4 @ 4 rpm
 
Thermal PropertiesMetricEnglishComments
Flash Point 27.8 - 31.1 °C82.0 - 88.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 45.0 - 80.0 min0.750 - 1.33 hourLay-up Time
Gel Time 10.0 - 17.0 min
@Temperature 25.0 °C
10.0 - 17.0 min
@Temperature 77.0 °F
Method POLYNT-22-TAS-TM-515.2, 100 g mass at 77°F, 1.8% United Initiators Norox® MEKP
 
Descriptive Properties
Sag ResistanceGood @ 20 mils
Thixotropic Index6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9208 / 231803

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.