MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Network Polymers Softflex® 0250
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: Softflex® Thermoplastic Elastomer Alloy

Information provided by Network Polymers Inc.

A. Schulman has acquired Network Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.890 g/cc0.890 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.017 cm/cm
@Thickness 3.17 mm
0.017 in/in
@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.015 cm/cm
@Thickness 3.17 mm
0.015 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow  0.20 g/10 min
@Load 2.16 kg,
Temperature 150 °C
0.20 g/10 min
@Load 4.76 lb,
Temperature 302 °F
Procedure A Condition C; ASTM D1238
 52.7 g/10 min
@Load 2.16 kg,
Temperature 190 °C
52.7 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Procedure A Condition E; ASTM D1238
 110 g/10 min
@Load 1.00 kg,
Temperature 235 °C
110 g/10 min
@Load 2.20 lb,
Temperature 455 °F
Procedure A Condition Q; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 20 - 3020 - 3010 second dwell; ASTM D2240
 24 - 3424 - 34Instantaneous; ASTM D2240
Tensile Strength, Yield 5.52 MPa800 psichs 20 in/min; ASTM D412
Elongation at Break 950 %950 %ASTM D412
Gardner Impact >= 36.2 J
@Temperature -30.0 °C
>= 26.7 ft-lb
@Temperature -22.0 °F
ASTM D5420
Tear Strength 19.3 kN/m110 pliASTM D624

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Network Polymers Softflex® 0150
CPT C-Flex® R70-001 Opaque Biocompatible TPE
CPT C-Flex® R70-003 Opaque Biocompatible TPE
CPT C-Flex® R70-046 Clear Biocompatible TPE
Network Polymers Softflex® 0350

PDIAM001 / 29839

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.