MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akro-Plastic Akroloy® PA GF 60 natural (2941) PA 66 + PA 6I/6T Dry, 60% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 60% Glass Fiber Filled

Material Notes: Description: Akroloy PA GF 60 natural (2941) is a 60% glass fiber reinforced polyamide blend with very high stiffness and strength, even in conditioned state. This material is listed at UL at 0.8 mm all colors HB. Applications are components with high dimensional stability, independent from moisture content. Akroloy PA GF 60 is an alternative for aluminum and zinc diecast alloys.

Features:

  • Good Dimensional Stability
  • High Stiffness
  • High Strength
Uses: Metal Replacement

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.72 g/ccISO 1183
Filler Content 60 %ISO 1172
Moisture Absorption 0.80 %
@Temperature 70.0 °C
Humidity, 62% RH; ISO 1110
Water Absorption at Saturation 3.0 - 3.5 %ISO 62
Linear Mold Shrinkage, Flow <= 0.0030 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cmISO 294-4
Spiral Flow 47.0 cmCross section: 7 mm x 3.5 mm
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 330 MPaH 961/30; ISO 2039-1
Tensile Strength at Break 275 MPa5 [mm/min]; ISO 527-2
Elongation at Break 2.5 %5 [mm/min]; ISO 527-2
Tensile Modulus 21000 MPa1 [mm/min]; ISO 527-2
Flexural Strength 405 MPa2 mm/min; ISO 178
Flexural Modulus 20000 MPa2 mm/min; ISO 178
Charpy Impact Unnotched 90.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 100 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 14.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 16.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 55.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Melting Point 255 °CDIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 245 °CISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 225 °CISO 75-2/A
Flammability, UL94 HB
@Thickness 0.800 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akro-Plastic Akroloy® PA GF 60 natural (2941) PA 66 + PA 6I/6T Conditioned, 60% Glass Filled
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled
Lubrizol Isoplast® 101LGF60NAT Engineering Thermoplastic Polyurethane Resin
Lubrizol Isoplast® 101LGF40NAT Engineering Thermoplastic Polyurethane Resin

PAKRO107 / 182694

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.