- flame retardant: V-0/3,2mm (UL 94)
- V-2/1,5mm (UL 94),softening temperature (VST/B 120)=185 °C
- also available in transparent colors
As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |