MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

AlphaGary Evoprene™ 3273 Standard SBS Thermoplastic Elastomer Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes:

Alphagary is part of Orbia.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 g/cc0.930 g/ccISO 2782
Viscosity Measurement 10
@Temperature 150 °C
10
@Temperature 302 °F
Kg/cm2; Macklow-Smith extrusion rheometer
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050ISO 892
Tensile Strength 5.50 MPa798 psiISO 37
Elongation at Break 800 %800 %ISO 37
100% Modulus 1.80 MPa
@Strain 100 %
261 psi
@Strain 100 %
ISO 37
Tear Strength 29.0 kN/m165 pliISO 34-B
Compression Set 32 %
@Temperature 22.0 °C,
Time 259000 sec
32 %
@Temperature 71.6 °F,
Time 72.0 hour
ISO 815
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 55.0 - 60.0 °C131 - 140 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not specified
 
Descriptive Properties
Bonds withPolystyrene
Chemical ResistanceAcetoneModerate
 Acids up to 80%Moderate
 AlcoholGood
 AlkalisGood
 Brake fluidModerate
 Chlorinate solventsPoor
 DieselPoor
 Ethylene glycolExcellent
 GasolinePoor
 Salt solutionGood
 Soda lyeModerate
 Water, 23°CGood
 Water, 95°CPoor
Ozone ResistanceFail - Crack100 pphm / 200 hrs / 20% strain
TransparencyTransparent

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Denka REOMER G G8250 Thermoplastic Elastomer, For Injection Molding
C.O.I.M. LARIPUR® LPR7025 Special Adipate Ester Polyurethane
Buckeye Polymers BP FLEX A 7010 UR Injection Grade TPE
BASF Elastollan® C 70 A HPM TPUR
Barlog Plastics KEBAFLEX SG 50 A.1 black TPE-S, Shore A50, black

PGARY9625 / 140418

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.