Borcycle NAV101L belongs to the Borcycle" M grade portfolio. It is a 100% post-consumer, transparent, gel-reduced Low Density Polyethylene recyclate (rLDPE) supplied in pellet form for high-end blown film applications. NAV101L is an ideal LDPE used where sustainability and circularity matter. NAV101L is a 100% post-consumer recyclate including a large part of recycled post-consumer plastic waste coming from pre-sorted municipal (household) waste. NAV101L is part of EuCertPlast certificate according to European Standard EN 15343:2007 (certificate available upon request). Due to the nature of recyclates, some variation in color can be observed between batches. Cas No. 9002-88-4 Typical characteristics: - High transparency with reduced gel content
- Available in homogenized 24-ton truckloads
- Low odor
- Filtration: 60 µm
Applications: - Collation shrink film
- Shrink film
- Lamination films for non-food contact primary packaging
- Non-food contact primary packaging
- Secondary and tertiary packaging where transparency and reduced gel content are key parameters
Information provided by Borealis AG |