MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Poco Graphite AXZ-5Q Industrial Grade Graphite
Categories: Carbon; Graphite

Material Notes: POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal graphite to each application. Post synthesis modifications enhance the original material to allow even greater flexibility for highly specialized conditions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 1.66 g/cc0.0600 lb/in³
Open Porosity 90 %90 %
Porosity 26 %26 %
Particle Size 5.0 µm5.0 µm
Pore Size 0.700 microns0.0276 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6969
Tensile Strength, Yield 34.0 MPa4930 psi
Modulus of Elasticity 9.00 GPa1310 ksi
Flexural Strength 52.0 MPa7540 psi
Compressive Strength 103 MPa14900 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00203 ohm-cm0.00203 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.60 µm/m-°C4.22 µin/in-°F
Thermal Conductivity 70.0 W/m-K486 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Poco Graphite ZXF-5Q Industrial Grade Graphite
Poco Graphite ACF-10Q Industrial Grade Graphite
Poco Graphite AXF-5Q Industrial Grade Graphite
Poco Graphite AXM-5Q Industrial Grade Graphite
Niobium C-103 (WC 103; 89Nb-10Hf-1Ti), Stress Relieved

CPOCO12 / 85589

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.