MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CoreLite PVC 60 Closed-Cell PVC Foam Sheet
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoplastic; Vinyl (PVC); PVC, Foam Grade

Material Notes: CoreLite® PVC is a closed-cell, cross-linked polymer PVC foam formulated for durability, strength, and high processing temperatures. It is compatible with multiple resins, adhesives, and processing techniques. It has a very low water absorption rate and excellent chemical resistance. Ideal for many lightweight composite applications in marine, transportation, wind energy, aerospace, and other industries.

Standard sheet dimensions are 45.27 x 96.45 inches. Property data reported parallel to the plane.

Information provided by CoreLite.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.75 lb/ft³10% Tolerance; ASTM D1622
Thickness 250 - 2750 mil
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 306 psiASTM D1623
Elongation at Break 13 %Shear; ASTM C273
Tensile Modulus 15370 psiASTM D1623
Compressive Strength 139 psiASTM D1621-10
Compressive Modulus 6.671 ksiASTM D1621-10
Shear Modulus 3.046 ksiASTM C273
Shear Strength 112 psiASTM C273
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.210 BTU-in/hr-ft²-°F
 
Descriptive Properties
ColorYellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CoreLite PVC 80 Closed-Cell PVC Foam Sheet
Overview of materials for PVC, Molded
CoreLite PVC 48 Closed-Cell PVC Foam Sheet
CoreLite PVC 100 Closed-Cell PVC Foam Sheet
Overview of materials for PVC, Foam Grade

PCOREL995b / 192468

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.