MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ EC-2086 Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: 3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 2634 psiEtched Aluminum Overlap, Salt Spray @ 35°C for 356 days
 2850 psiEtched Aluminum Overlap, 100% RH @ 49°C for 356 days
 3328 psiEtched Aluminum Overlap, 100% RH @ 49°C for 180 days
 3670 psiEtched Aluminum Overlap, 100% RH @ 49°C for 90 days
 4140 psiEtched Aluminum Overlap Freon 22 Resistance, 60 days @ RT
 4225 psiEtched Aluminum Overlap Freon 22 Resistance, 1 year @ RT
 4470 psiEtched Aluminum Overlap Freon 22 Resistance, 30 days @ RT
 4650 psiEtched Aluminum Overlap Freon 22 Resistance, Control
 4692 psiEtched Aluminum Overlap, Salt Spray @ 35°C for 180 days
 4720 psiEtched Aluminum Overlap, 100% RH @ 49°C
 4830 psiEtched Aluminum Overlap, Salt Spray @ 35°C for 90 days
 5064 psiEtched Aluminum Overlap, Salt Spray @ 35°C
 5710 psiEtched Aluminum Overlap, Hydraulic Oil @ RT
 5784 psiEtched Aluminum Overlap, Tap Water @ RT
 5962 psiEtched Aluminum Overlap, Tap Water @ RT for 90 days
 6024 psiEtched Aluminum Overlap, White Gas @ RT
 6100 psiEtched Aluminum Overlap, Tap Water @ RT for 356 days
 6152 psiEtched Aluminum Overlap, Tap Water @ RT for 180 days
 130 psi
@Temperature 177 °C
Solvent Wiped Cold Rolled Steel Overlap
 480 psi
@Temperature 121 °C
Solvent Wiped Cold Rolled Steel Overlap
 500 psi
@Temperature 177 °C
Etched Aluminum Overlap
 2200 psi
@Temperature 121 °C
Etched Aluminum Overlap
 2360 psi
@Temperature 82.0 °C
Solvent Wiped Cold Rolled Steel Overlap
 2700 psi
@Temperature 24.0 °C
Solvent Wiped Cold Rolled Steel Overlap
 3000 psi
@Temperature -55.0 °C
Etched Aluminum Overlap
 3340 psi
@Temperature -40.0 °C
Solvent Wiped Cold Rolled Steel Overlap
 3500 psi
@Temperature 232 °C
Bond Line
 4300 psi
@Temperature 218 °C
Bond Line
 5000 psi
@Temperature 82.0 °C
Etched Aluminum Overlap
 5000 psi
@Temperature 24.0 °C
Etched Aluminum Overlap
 5300 psi
@Temperature 204 °C
Bond Line
 5500 psi
@Temperature 11.0 °C
Bond Line
 5500 psi
@Temperature 177 °C
Bond Line
Peel Strength 50.0 pliSolvent Wiped T-Peel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.60e+14 ohm-cm
Surface Resistance 1.00e+17 ohm
Dielectric Constant 10.8
@Temperature 23.0 °C
 11.4
@Temperature 60.0 °C
Dielectric Strength 123 kV/in
Dissipation Factor 0.016
@Temperature 23.0 °C
 0.228
@Temperature 60.0 °C
Arc Resistance 34 sec
 
Thermal PropertiesOriginal ValueComments
CTE, linear 47.0 µm/m-°C
@Temperature -18.0 - 27.0 °C
Thermal Conductivity 2.98 BTU-in/hr-ft²-°F
 
Descriptive Properties
AppearanceGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM34628 / 169375

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.