MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Anderman Ceramics EAZ 20 Zirconia Toughened Alumina
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes.

Key Words: Al2O3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.30 g/cc
Open Porosity 0.00 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 42000 psi
Flexural Strength 65000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+9 ohm-cm
@Temperature 600 °C
 1.00e+14 ohm-cm
@Temperature 20.0 °C
Dielectric Constant 10.6
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.30 µm/m-°C
Thermal Conductivity 27.0 W/m-K
@Temperature 20.0 - 100 °C
Maximum Service Temperature, Air 1500 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 77 %
ZrO2 23 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
Anderman Ceramics EA995 Sintered Alumina, 99.5%
Anderman Ceramics EM80P Corundum
Anderman Ceramics EZM 96 Zirconia, 96.5%, Magnesia-Stabilized
Aremco AREMCOLOX™ 502-1900-ZTA Dense Zirconia-Toughened Aluminum Oxide

CANDER17 / 104652

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.