MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Nouryon Trigonox 99-W50 Cumyl peroxyneodecanoate
Categories: Other Engineering Material

Material Notes: Initiator (75% active ingredient in water) for (co)polymerization of vinyl chloride and vinylidine chloride.

CAS number: 26748-47-0

EINECS/ELINCS No: 247-956-7

Applications: Trigonox 99-W50 is used as an initiator for the suspension and mass polymerization of vinyl chloride between 40°C and 65°C. Trigonox 99-W50 is often combined with less active peroxides such as peroxydicarbonates (e.g. Perkadox 16) or diacylperoxides (e.g. Laurox) to increase reactor efficiency. Reasons to use a water-based peroxide emulsion instead of a solvent-based peroxide are the following: enhanced safety, easy to use (pumpable) in ‘closed reactor technology’, easy to dilute with water

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc
@Temperature 0.000 °C
0.0354 lb/in³
@Temperature 32.0 °F
Half-life  0.100
@Temperature 76.0 °C
0.100
@Temperature 169 °F
[hr]
 1.00
@Temperature 56.0 °C
1.00
@Temperature 133 °F
[hr]
 10.0
@Temperature 38.0 °C
10.0
@Temperature 100 °F
[hr]
Brookfield Viscosity 200 - 2000 cP200 - 2000 cPLVT, spindle #3, 5 rpm
Storage Temperature -25.0 - -20.0 °C-13.0 - -4.00 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 10.0 °C50.0 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceWhite emulsion
Assay49.0-51.0 %
Content (%)5.22Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1146 / 286669

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.